By HJLBX
Date 07-12-2016 06:08
Edited 07-12-2016 06:13
jdschauerman...
You're not crazy - yet.
I have been in contact with AWS in regards to this matter. Their explanation as to the cause of text errors is typographical and layout errors made by the printer.
There are more than just a few errors in the AWS study materials - both in the required and suggested body of knowledge texts as well as the online training.
Incorrect formulas, mis-located images, missing\incomplete sentences, quiz questions that do not contain the correct answer, etc.
The older versions of the WIT text and study guide (quizzes) have more errors than the latest version - but they all have overt errors.
The best that you can do is catch and make a mental note of the errors as you study.
Someone that doesn't pay attention - well - it could mean the difference between that person passing or failing the CWI exam.
Considering the cost of all the materials - and the fact that some of us have no resources other than the AWS study materials to learn - it is frustrating and sometimes downright infuriating - but it just is what it is...