As most of you oilfield hands know most rigs are in remote locations, my rig is 120 miles out in the gulf, I needed a 4"sch. 80 "tee" to repair a washout on a saltwater line, most of the time I have to fab my fittings. So what you guys think?
Looks good to me like you said 120 miles out not like you can run to town and pick 1 up
Looks great!! You can tell this isnt your first day on the job.
That sure is pretty. Good work
Hojo, who are you working for if you don't mind me asking, I'm up in the Jackson area?
Oil field is that way even when on land and it's only 5 miles to town they will want you to fab something that takes 1/2 a day to make when it only cost 20.00 in town just so they can save 20.00 lol wierd i know but i never complain just say yes sir and get after it kinda makes me feel guilty sometimes
Nice work......Of course I know very little about pipe.
When you came around the corners were you going up or down? What rod? Thanks for considering my simple question!
Jon
root and hot pass 1/8 6010 downhill, filler and cap 1/8 7018 uphill, all on 4" sch. 80 I also have a rig truck and do alot of work when i'm off, this is part of a supply header I worked on for a co2 plant.
By Superflux
Date 02-07-2009 08:58
Edited 02-07-2009 09:10
Sure is an awful big 4" compared to that jack stand.
Nice work. Even your initials are plumb and square. Craftsman.
It looks like 6" pipe to me.
the pic with my stamp is 6" / with 2 6" to 2" eccentric reducers all sch. 80.