- - By hojopens3 (**) Date 02-02-2009 22:19
As most of you oilfield hands know most rigs are in remote locations, my rig is 120 miles out in the gulf, I needed a 4"sch. 80 "tee" to repair a washout on a saltwater line, most of the time I have to fab my fittings. So what you guys think?
Attachment: hojoworkpics.jpg (192k)
Parent - - By raftergwelding (*****) Date 02-02-2009 23:03
Looks good to me like you said 120 miles out not like you can run to town and pick 1 up
Parent - - By Tim655 (*) Date 02-02-2009 23:16
Looks great!! You can tell this isnt your first day on the job.
Parent - By hojopens3 (**) Date 02-02-2009 23:19
thanks Tim
Parent - By hojopens3 (**) Date 02-02-2009 23:19
thanks shad
Parent - By OBrien (***) Date 02-03-2009 03:08
That sure is pretty.  Good work
Parent - - By ANDY LARKINS (*) Date 02-03-2009 17:16
Hojo, who are you working for if you don't mind me asking, I'm up in the Jackson area?
Parent - By hojopens3 (**) Date 02-03-2009 22:38
work for blake offshore
Parent - By raftergwelding (*****) Date 02-04-2009 15:14
Oil field is that way even when on land and it's only 5 miles to town they will want you to fab something that takes 1/2 a day to make when it only cost 20.00 in town just so they can save 20.00 lol wierd i know but i never complain just say yes sir and get after it kinda makes me feel guilty sometimes
Parent - - By fbrieden (***) Date 02-04-2009 15:17
NICE!
Parent - - By JMCInc (**) Date 02-06-2009 17:20
Nice work......Of course I know very little about pipe.
When you came around the corners were you going up or down? What rod? Thanks for considering my simple question!
Jon
Parent - - By hojopens3 (**) Date 02-07-2009 02:04 Edited 02-07-2009 02:35
root and hot pass 1/8 6010 downhill, filler and cap 1/8 7018 uphill, all on 4" sch. 80 I also have a rig truck and do alot of work when i'm off, this is part of a supply header I worked on for a co2 plant.
Attachment: 09-11-08_1130.jpg (0B)
Parent - By JMCInc (**) Date 02-07-2009 02:42
Thank you.
Parent - By Superflux (****) Date 02-07-2009 08:58 Edited 02-07-2009 09:10
Sure is an awful big 4" compared to that jack stand.
Parent - - By Oregon Jake (**) Date 02-07-2009 09:14
Nice work.  Even your initials are plumb and square.  Craftsman.
Parent - - By thewelder (***) Date 02-07-2009 21:14
It looks like 6" pipe to me.
Parent - By hojopens3 (**) Date 02-08-2009 01:08
the pic with my stamp is 6" / with 2 6" to 2" eccentric reducers all sch. 80.