- - By JNolan Date 02-10-2009 18:56
I need more info on this certification. I had some training in college a long time ago, and am curious as to the depth and breadth of this exam. Will the pre study like that of the CWI exam be enough or should I be looking at additional training else where? I am located in Michigan so if you know any good resources here that would be a tremendous help? Thank you. JRN
Parent - By Terry Vititoe 2 (*) Date 02-16-2009 10:43
Hey, I took the exam in June of last year, and passed; it was tough, a lot of code review (acceptance & reject). Study ASTM E-1742,E-94, D1.1, API, & ASME V for starters. I'm not sure, but I think that they are running at about a 50% failure rate good luck