Tight cracks can easy be missed on RT, so can lack of fusion.
Is RT >> PWHT >> RT-ASR required by project specs?
To the best of my understanding MT (or any NDT) after PWHT is not mandatory for P1 materials, unless of course if it is part of the specified random control.