If I understand the question, there is no maximum size limitation except for lap joints. The T-joint is not a lap joint, so the size limitations for the fillet weld often cited by people, i.e., equal to the thickness of the member for materials under 1/4 inch thick and 1/16 inch less than the thickness of member for materials 1/4 or thicker, doesn't apply.
best regards - Al