I need to know the best way to weld ductile cast iron to ductile cast iron. Is there a procedure that i can find? What welding rod, parameters, gas, etc.?
Just a curious question. Why do you need to weld a ductile cast iron pipe to another ductile cast iron pipe? Ductile cast iron pipes are normally joined together by the "bell and spigot" procedure.