Up Topic Welding Industry / Metallurgy / A106 Gr.B NACE MR0175 minimum requirements
- - By Maad Date 03-20-2018 19:28
Hi everyone
    Can anyone tell me the minimum hardness for carbon steel >>>pipe A106 Gr.B NACE MR0175 ? because in 15156  just give us the maximum limit (22HRC) . Also what is the minimum requirements for NACE MR0175 from the side of chemical composition and other mechanical properties . thanks alot for everyone
Parent - - By RomanMet Date 03-27-2018 23:09 Edited 03-27-2018 23:43
If the material have cold strain equivalent to  15 % or les, provided the hardness in the strained area does not exceed 190 HBW, this is another consideration to take into account

Hardness min

Must be according to ASTM A106 gr B. But we estimate the value of hardness according to your effort to stress & ASTM 370. this could be estimate the hardness according to Tensile Strength min (60 Ksi) Table 3 Approximate Hardness 123 HB min. The min hardness value is not a requirement but it is a reference value.
Parent - By Maad Date 03-28-2018 13:02
Thank you very much RomanMet