Hello,
My question is, If a PQR is tested to API 1104 on a Lap joint fillet weld does that also qualify for the branch fillet?
"To weld the test joint for a fillet weld, a fillet weld shall be
made to one of the configurations shown in Figure 10, following
all the details of the procedure specification" They are using the 19th ed..
I cant find anything that clarifies that qualifying to 1 of the configs in Fig 10 qualifies for both or just the one that was tested on the PQR?
To me it makes sense that the Branch would qualify for both but not the other way around...
Thanks