We want to use electroslag process for cladding.
Have any of you experience with this process?
What are the critical parameter and the most common defects?
Thanks in advance for your responses.
Javier Sanchez
Santander
ESPAÑA
By
PhilThomas
Date
03-03-2005 13:29
What materials are you wanting to clad? (e.g. what is the base material and the desired overlay material?)
Stoody has developed and patented such a process; a brief description is here:
http://www.thermadyne.com/newsprodspotdetail.asp?div=stdy&id=165
By
javiersanchez
Date
03-03-2005 14:06
- We have to clad with INCONEL a piece of 500mm of thicknes, diameter of 4 meter made of SA-508 Gr3 Cl2 (P3)
By
PhilThomas
Date
03-04-2005 13:03
The Thermaslag process was developed for welding 400-series stainless overlays on steel mill rolls. I don't know of any work that has been done with cladding Inconel using electroslag. It might be possible.
By
GRoberts
Date
03-04-2005 21:02
http://www.aws.org/wj/nov02/feature2.html
Topic
Welding Industry
/
Technical Discussions
/ Electroslag process
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill