Tom, Marty is absolutely correct, the PQR does not qualify for other P numbers. However, if the welder qualifies, then for performance qualification purposes he may be qualified. Regardless of the above, the mandated "complete weld w/o interruption and stress relieve immediately after weld" would be considered an Essential Variable and MUST be followed./