By JBS
Date 01-15-2007 15:34
I'm looking for some techalloy Nickel 61 ( NI208 ), .045 DIA. , mig weld wire for immediate purchase . If you have any available in stock it would be much appreciated . Techalloy will not be releasing another shipment of wire until FEB. 15th so I am looking for any that might be on shelf . I can be contacted at the following email address . jbs20003@msn.com Thanks for your time !