A follow up to one of my posts that so many gave me great opinions on.ITwas in refer to my having to weld 304 stainless to carbon steel.I used 309/035 stainless wire.I used a back step method to weld the plate that was about 2'.I also used trimix for the sheilding gas.I was very impressed with the out come.The weld it self was married to the carbon with ease.It was a really clean an a great looking weld.Thanks all for your opinoins,
monsoon12