Does anybody know where to buy a vacuum box for testing welds on tank floors and floor to shell welds? Thanks, Henry
By
hogan
Date
02-07-2007 19:40
this is a good site for ndt equipment
http://www.macraesbluebook.com/search/product_company_list.cfm?Prod_Code=7805300
By
CWI555
Date
02-07-2007 22:01
You could make one. It doesn't take much, just have to have calibrated gauges to document your vacuum.
By
MNSTRBLDR
Date
02-07-2007 22:19
We tried that a while back. Does anybody have a diagram of how the guage and air is supposed to be connected with pipe size etc.? Henry
Topic
Welding Industry
/
Inspection & Qualification
/ vacuum box tester
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill