- - By hogan (****) Date 02-14-2007 23:00
i'm looking at d1.5(2002) and there look like there is a conflict with 1.3.1 stating that smaw is the only process that is prequalified. if compared to 2.7 and 2.8. i'm looking to do a small amount of fillet weld work (fcaw-g). can someone enlighten me?
Parent - - By Joseph P. Kane (****) Date 02-14-2007 23:24
The FCAW Process is not prequalified.  Some joints are prequalfied, but that is not the same as the welding process.  Sorry.
Parent - By hogan (****) Date 02-15-2007 14:43
i can see i need more sleep. too many audits at the same time.
Parent - - By HgTX (***) Date 02-16-2007 17:02
Technically speaking, the joints aren't "prequalified" either; they're "standard" (see C2.7.1).  The use of this term "prequalified" to describe those joints is a source of confusion.

Hg
Parent - By Joseph P. Kane (****) Date 02-16-2007 20:44
I stand corrected.