- By metalcoat (*) Date 02-22-2007 18:33 Edited 02-25-2007 10:18
Hello!, I am from India. I would like to know which welding electrode for MS welding (SMAW) will have the specification as - E/6 31x413 as per Indian Standard IS-815? And which make of it will be better for welding mild steel plates?