We are working on fillet PQR's. We have performed the 3 macro's as needed. My question is do we now need to perform the bend test or is this only if the welder needs to be certified? I am looking at table 4.4.
By
brande
Date
03-03-2007 05:51
Trusting my very rusty memory....no code book here at present.
PQR's are qualified by macroetch alone.
Welder quals (performance quals)
are qualified by both break test and macroetch.
Check it out, let me know!!
Good Luck
brande
Topic
Welding Industry
/
Inspection & Qualification
/ Fillet Weld test per D1.1
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill