- - By Ian Date 02-20-2001 08:31
Does anyone have any information, or experience, in Mig Brazing ? Can this process be used with 'hobby' Mig sets or is it a very specialised form of brazing. I have found some info on consumables from a company called Daishin Industrial Co Ltd (on the internet) but its in Japan. Are there any suppliers of a similar product in the US or UK ?

Any info would be greatly appreciated.

Thanks in advance

Ian

( PS. The title should have read GMAW (as corrected) not SMAW - as a Brit these terms sometimes confuse (thats my excuse anyway !)
Parent - By leffe Date 04-20-2001 16:53
Since brazing needs less heat, it can be done with relatively light equipment. Give it a try before buying new equipment. Else, you can look for Fronius Equipment. They have demonstrated me a dedicated MIG brazing machine.

Leffe.