Is there a equation or something that states, what's the max size fillet weld that can be made in one pass on any size mild steel according to AWS standards?
By
QCCWI
Date
04-10-2007 18:32
AWS D1.1 lists maximum fillet weld size by process Section 3.7.3.2 SMAW 1/4" SAW 5/16" GMAW/FCAW 5/16"
By
hogan
Date
04-10-2007 18:46
also table 3.7
By
surprisej
Date
04-11-2007 04:46
Thanks guys
Topic
Welding Industry
/
Technical Discussions
/ Fillet weld
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill