- By steeltailor Date 04-28-2007 07:31
SteelTailor P is a portable CNC Cutting Machine.It can cut any complex
plane figures as the large-sized gantry CNC cutting machine and
support both flame torch and plasma cutter. It is affordable for all
enterprises and workshops. The compact design and rational structure
make it lightweight,small size and easy to move. It is usable both
indoors and outdoors.

By using high quality controllers in its automation system and
antimagnetic materials in its housing, SteelTailor P guarantees a
reliable and stable CNC operation.

The application of the most up-to-date CNC technology allows
independent programming from numerical control . equipment failure and
maintenance difficulty are reduced.

The integration of FastCam cutting software makes drawing, nesting and
cutting simple and efficient. The software provides hight leves of
material utilization & optimization.

More info:
Http://www.SteelTailor.com
Colin.lai@SteelTailor.com
Up Topic Welders and Inspectors / Welding Equipment Classifieds / portable CNC Cutting Machine

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill