- - By defaced (**) Date 04-30-2007 19:58
I'm taking an introductory class on UT and RT and am finding that the instructors notes are far from sufficient.    I'd like to find something along the technical level and scope of the Welding Handbooks but for UT and RT.  I realize there probably isn't a single text that covers the two different topics in this maner, that's fine.  Any suggestions?
Parent - - By jwright650 (*****) Date 04-30-2007 20:13
defaced,
Is there anything that I can help with regarding UT?
Parent - By defaced (**) Date 05-02-2007 14:43
Right now I don't have anything specific, but as I dig a little deeper I'm sure I can field some questions to you. 
Parent - - By hogan (****) Date 04-30-2007 20:51
general dynamics has a good line of ndt books. ct-6-4 for one of the ut books, there are a total of 3 books per method not sure of the #'s for other two or for rt
Parent - - By CWI555 (*****) Date 05-01-2007 02:02
I believe it's 4 four RT
Parent - - By dmilesdot (**) Date 05-01-2007 13:45
There is a website called Radiated Fields of Ultrasonics..check it out.
Parent - - By Bill M (***) Date 05-01-2007 17:26
Kodak printed a very informative Radiography manual called "Radiography in Modern Industry" :  212 pages

.pdf Copy free on-line here:

http://www.kodak.com/eknec/documents/87/0900688a802b3c87/Radiography-in-Modern-Industry.pdf
Parent - - By thcqci (***) Date 05-01-2007 20:55
I have an older hard copy of this.  Thank you for posting that link.  Another site that has been referenced on this forum before is...   http://www.ndt.net/article/az/ut_idx.htm

There are a couple of versions of the GE books mentioned above.  One is much more basically delivered for self study and one geared toward classroom presentation which goes into more depth.
Parent - - By defaced (**) Date 05-02-2007 14:40
Thanks for all of the help everyone!  Both the intro section about UT on NDT-ed and that Kodak PDF look like they'll be perfect for what I'll need. 
Parent - By Inspectroleum (*) Date 05-07-2007 17:26 Edited 05-07-2007 17:29