Anyone can help me if wps for pipe A106 GrB is qualify for welding A53 Gr.B pipe. Both are in P-1 and Gr-1. Thks
By
jon20013
Date
05-03-2007 11:50
If you are working under ASME Codes then your WPS is most certainly qualified to weld the A53, Gr. B. In fact even outside of the ASME world I believe the answer would be the same for any Code I am familiar with.
Topic
Welding Industry
/
Technical Discussions
/ WPS ASTM A106 Gr.B For A53 Gr.B Pipes
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill