What are the causes of lack of sidewall fusion, weld bead undulation, and erratic arc behaviour in the root run and hot pass in tandem welding of grooves
By
Joseph P. Kane
Date
05-19-2007 13:49
With the limited information given here, and assuming you are talking about SAW, magnetic arc blow sounds like the problem.
By
isaiah
Date
05-20-2007 07:41
Thanks Joe, I am actually working on tandem MIG/MAG welding
Topic
American Welding Society Services
/
AWS Learning & Education
/ tandem welding
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill