- - By bhiltz (**) Date 03-10-2001 23:36
ANYONE KNOW WHERE I CAN FIND SOME INFORMATION ON PULSE MIG , FOR WELDING GAUGE THICKNESS STAINLESS STEEL? ANYONE HAVE ANY EXPERIENCE WITH PULSE MIG ON STAINLESS?
Parent - - By DGXL (***) Date 03-11-2001 18:28
Miller has an excellent book on the subject: GMAW-P Pulsed Spray Transfer. There is a lot of good information in the AWS Welding Handbook - Volume 2 as well.
Parent - By 357max (***) Date 03-12-2001 18:49
That Miller book on Pulse is great! Miller distributors can get it for you. The stock number for ordering is #168 336. Also look at their GMAW book #151 682. The cost was only 5 for the Pulse and 15 for the GMAW. Money well spent.
Parent - By dee (***) Date 03-12-2001 18:49
log on to WELDREALITY.COM... ask specific questions under the OPINIONS bulletin board... should find answer within one day or so