- - By drifter57 (**) Date 07-12-2007 14:00
Quick question for the Alum guys out there. Looking for personal peferences comparing Radnor to Harris for filler mat. Numbers the same, do you prefer one brand over the other and if so why. Thanks in advance for any info.
Parent - - By Greg G. (**) Date 07-12-2007 15:27
What is the application. Make sure if your part gets anodized you don't use 4043 it will not anodize. It will turn black.  To much silicone in the rod. Use 5356 it will anodize. All the rods are pretty good for my money.
Parent - - By drifter57 (**) Date 07-12-2007 16:08
Greg, 4043 rod. Just wondering if there is a preference on  the name brands themselves.
Parent - By Greg G. (**) Date 07-12-2007 17:36
Either will work.
Parent - By 357max (***) Date 07-12-2007 18:36
Check with your Radnor distributor, Radnor doesn't make the wires they only package as a lot of retailers do.