- By UWMSE Date 07-20-2007 15:35
We are researching friction stir spot welding of Aluminum to Copper and copper to aluminum and the threaded pin is becoming clogged with material after several welds, hence preventing mixing.  Does anybody have any suggestions as to a good cleaning step to remove the material from the threads?  Thanks.