Welding Industry
/
Inspection & Qualification
/ detection of unbonds in brazed assemblies
By
prasad
Date
07-24-2007 23:25
What is the most effective NDT method to detect unbonds in brazed assemblies.
By
hogan
Date
07-25-2007 13:46
typically it would be strait beam ut
By
prasad
Date
07-26-2007 14:51
Yes I tried Straight beam UT . Tks
Topic
Welding Industry
/
Inspection & Qualification
/ detection of unbonds in brazed assemblies
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill