- - By pointmayer 2 Date 07-25-2007 14:44
hi just wonering if anyone has a word copy of a welding visual inspection report
Parent - - By 803056 (*****) Date 07-25-2007 21:55
Nearly every job is different fom the last one you worked on. Each code has different attributes on which you base acceptance or rejection of the welds. Each client may have different information that has to be included in the report. The result is that you may have to develop several different formats to address the attributes that are evaluated. With many inspectors using the computer, there's no reason not to tailor the report to job specific needs.

Best regards - Al
Parent - By fbrieden (***) Date 07-26-2007 03:09
That's what I do!