By jgks
Date 04-06-2001 02:28
Yes I would be interested as well.
Most of the jigs I've seen were Aluminum plates drill and tapped
to accept the tubing holddowns. However this only allows you to
tack. Then another jig is used to hold the piece and reduce
expansion while completing the joint welds.
If anyone has plans for could direct me that would be great.
jgks