When qualifying a double "Vee" groove butt joint weld procedure, is the filler metal considered "backing" material with respect to AWS welding codes?
By
RonG
Date
03-28-2001 01:30
Good question!
If you turn it over first and weld the groove closed then flip it over and back grind your weld it is called a "Backing Weld" and it serves as a back up. But is it backing. I should think it would be the same as backing.
Topic
Welding Industry
/
General Welding Discussion
/ Filler Metal and Backing material
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill