- - By Carbon Arc Junkie (*) Date 09-14-2007 03:14
Have to weld some hutches to the webing of a beam.  Which is the best procedure... using .045 or .030?  And which wire type... Hard or Flux?

Thanks in advance.

"Too shaky and old to do anymore Tig"
Parent - - By darren (***) Date 09-14-2007 04:38
out of position hard wire is too hard without pulse. fluxcore any size wire will do. if you could explain a hutch and give a little more info could dial it all in. does the weld have to be pretty or just functional. like i say a little more info would make it so that we could give you the exact info.
i noticed this is only your second post welcome to aws

darren
Parent - By Carbon Arc Junkie (*) Date 09-14-2007 04:57
Darren,
   I'm glad to be here.  I posted this in two places, and didn't mean to. I got some of the answers I needed, and will be working hard this weekend to prefect it. 