Not logged inAmerican Welding Society Forum
Forum AWS Website Help Search Login
Up Topic Welding Industry / Technical Discussions / HELP! 17-4 SS weld info?
- - By meanstreak (*) Date 10-10-2007 23:55
We have a heat treated 17-4 fabricated high performance marine rudder. It has some cracks where the shaft joins to the blade. Would like some repair data ,ie;tig rod to use, pre heat , reheat treating etc. Thanks in advance four help.  Nate
Parent - By Lawrence (*****) Date 10-11-2007 08:33
Be sure to make note of thermal conditioning treatment options.

http://www.hightempmetals.com/techdata/hitemp17-4PHdata.php
Up Topic Welding Industry / Technical Discussions / HELP! 17-4 SS weld info?

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill