- - By weld123 Date 10-15-2007 03:33
      can anyone please describe to me whats all involved in getting certified to weld rebar.     i gather there are differnt types of joints and dont know if theres one test to qualify for all or more than one type of joint.     is there a standard procedure written like the strucral plate test.    also what ways is the rebar speciman tested.      thanks
Parent - - By jerrykroll (**) Date 10-15-2007 16:19
AWS D1.4 Reinforcing Steel.

Indirect Butt Double Flare Bevel (bar to plate) covers most joints except full pen. Qualify the procedure as you qualify the first welder - visual and macro etches.
Parent - - By swsweld (****) Date 10-16-2007 03:03
Jerry what welding process are we talking about? I don't have D1.4. Thanks.
Parent - - By jerrykroll (**) Date 10-17-2007 00:02
Generally speaking - SMAW or GMAW - makes little difference
Parent - - By swsweld (****) Date 10-18-2007 02:46
A couple of weeks ago a civil QC on our job stopped us from tacking rebar to our wall sleeves to help support them. Other jobs in the past had no problem with it was not sure if present QC had code to back him or if it was just his opinion that tacking rebar was code violation.
Parent - - By jerrykroll (**) Date 10-20-2007 13:58
From D1.4-

5.4 Tack Welds

"Tack welds that do not become a part of permanent
welds shall be prohibited unless authorized by the Engineer.
Tack welds shall be subject to the welding requirements
of the code, including preheat, electrode selection,
and discontinuity acceptance criteria."
Parent - By swsweld (****) Date 10-21-2007 03:43