Is there a specific way to make correctios to a Welder Qualification Test Record. More specific the dates. There was a typo problem with the software that originally produced the documents. Can the date be crossed out and the actual date penned in with initials? Reason I am asking is dates say 1904 when it was actually 2004.
I don't believe anyone would put you in the stocks for making the correction as you noted. A single line struck through the error, a correction, initialled, with a date of the correction is the typical means of making the correction.