By LaserJock
Date 11-16-2007 21:29
Edited 11-16-2007 21:33
Anybody try or have experience in welding this material (BioDur CCM Plus alloy - Carpenter trade name), any process?
Alloy described as follows; Carbon - 0.20 to 0.30%, Chromium - 26.00 to 30.00%, Molybdenum - 5.00 to 7.00%, Cobalt - "Balance", Nitrogen 0.15 to 0.20%