ok i got a 250d and im looking for mig capabilty. ive looked at the millers and seems like the only thing they have that i could use is the 8 and 12 VC exstreme. im trying to get lincolns site up but it doesnt want to load for some reason. but they have a new ln25 pro. what i need is everybodys input or opinion on these two suitcases and their compatabilty with my rig. any known problems? likes dislikes? thanks in advance guys
Parent - - By mody454 (**) Date 11-25-2007 17:04
says the ln25 pro does pulse too
Parent - By DaveBoyer (*****) Date 11-28-2007 04:19
I think for that LN25 to do pulse You will have to hook it up to a pulse capable power suply, not just any old welder.
Parent - - By Justin O (**) Date 11-27-2007 06:07
I have and like how the 12vs is set up.
Parent - - By mody454 (**) Date 12-09-2007 19:43
the 12 vs can hook to any welder right you dont have to have 14 pin?
Parent - By DaveBoyer (*****) Date 12-10-2007 03:36
They don't use any controll cord at all, hook to any DC machine.
Parent - By makeithot (***) Date 12-13-2007 02:59
I us a miller 12VS and have no trouble with it at all it works great and makes money day in day out, nice unit.