I've been told that 7 series aluminum is near impossible, or at least fairly difficult to weld.
I'm looking at 7005-T5, as well as 7039-T64 tubing. Does anybody have any experience with these? Difficulty, suggested filler, etc. Most of my experience is with 6061.