jlewontin
Date
04-25-2001 18:37
Based on fume measurements from TIG welding 4130 steel, I would like to ballpark the fume levels to be expected from TIG welding 7005 Aluminum in a similar setup. Any experience or ideas on this?
By
stan ford
Date
04-25-2001 20:43
See TWI's "Welding Fume Tutor" software available from C-spec (www.cspec.com).
Topic
Welding Industry
/
Technical Discussions
/ Fumes
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill