By milan
Date 01-09-2008 07:18
I'm searching for brazing alloys wich MAY NOT contain the following elements:
Zn/Cd/Pb/P/S..
we use now Incusil en cusiltin...
Si is not our favorit, accordig the literature:
the joint is highly vaccum thight e-10Pa
temperature between 400-650 Celcius, and as a preform 50 micron (0,02")
what are the possibilties?