- By TolgaKantaroglu (*) Date 01-10-2008 21:36
Dear All,

Do you have any filler wire recommendation for the subject combination. Processes are GTAW+SMAW and I am thinking to use ER NiCR-3 and E NiCrFe-2. ER 309L and E2209 are also possible but what would be the best? I will appreciate your earliest recommendation.

Thanks and regards,

Tolga