- - By norsky63 (**) Date 01-13-2008 16:09
I just fired up my trusty old red face and it has no output. It was sitting outside here in northern mn.for a couple of months. She worked great when I parked her but now nothing.  I checked the brushes and their fine. only 2.5 volts output .any help would be great!!
Parent - - By texasrigwelder (**) Date 01-13-2008 20:50
wat about the exciter brushes, just take the cover off hook ur stinger and ground together and poor some hot water on em some rats could of also maybe climed in and chomped on some wires
Parent - - By norsky63 (**) Date 01-13-2008 21:36
I found the problem the commutator on the exciter was dirty. I'm gonna get a cleaner n fix r right. Thanks for the reply.
Parent - - By KSellon (****) Date 01-14-2008 22:37 Edited 01-15-2008 23:15
SA200 wiring schematic. Ok I got it to load, but it is small. Good luck to all.
Attachment: SA200-SCHEMATIC.bmp (211k)
Parent - - By norsky63 (**) Date 01-15-2008 00:23
  k  the wiring diagram would be great I'm gonna build my own remote could you e mail to me at deanprestby@hotmail.com ?  thanks
Parent - - By welderdude (**) Date 01-15-2008 00:49
I'd like to see how to do that!
Parent - - By norsky63 (**) Date 01-15-2008 12:35
i'll show ya when i get it done it isn't too hard
Parent - By KSellon (****) Date 01-15-2008 14:26
It's not too hard, but for the time it's just as good to get one from Cable Remotes.
Parent - - By KSellon (****) Date 01-15-2008 23:16
I will get a hand drawn schematic in uploaded as soon as possible.
Parent - By norsky63 (**) Date 01-16-2008 03:10
I got it thanks alot !!!