- - By 52lincoln (***) Date 01-17-2008 01:34
what is the appendix c test
Parent - - By James Corbin (**) Date 02-05-2008 17:54
D1.1 Annex C (Normative) is "Weld Quality Requirements for Tension Joints in Cyclically Loaded Structures". See section 6 Part C RT acceptance Criteria 6.12.2.1 and 6.12.2.5. & Illustration Annex C.
Could you mean part B of the CWI practical test??-- http://files.aws.org/certification/docs/partb2006.pdf
Parent - By 52lincoln (***) Date 02-05-2008 22:38
thanks for the reply,they tould me finally it was a bend test and you was allowed one break