Can anyone give me the specific differences between these standards? I have heard ISO vs SNTC-1A are very similar. Is it too much to list??:-) Thanks--
ISO 9712 is ISO's attempt to unify and standardize all the various certification schemes world wide. ASNT ACCP program is ISO 9712 compliant to my knowledge. TC1A is a recommended guideline, subject to modification by the employer.