- - By IDIEM Date 01-31-2008 16:57
Please, can anyone tell me about of the porosities acceptance criteria in AWS D1.3 code. I'm doing inspections and need know about this question.

Abraham.
Parent - - By jwright650 (*****) Date 01-31-2008 17:22
I don't have a current copy of D1.3, but maybe if you take a look at AWS D1.3 paragraph 6.1.1 and if the welds meet those four criteria it should be deemed as acceptable. Make sure you have a current copy if that is what you are inspecting to.
Hope this helps.
Parent - By IDIEM Date 02-01-2008 13:47
Thank you for your atention. I am a chilean and it's for me very important to know all about welding.

Abraham.