/ Remote amperage controls
By
Shooter71
Date
02-05-2008 22:41
Does anyone have experience with the weldtron pipeliner hand control? And what remotes are people using besides the stock lincoln one for sa200's?
By
cpopham
Date
02-06-2008 01:14
I use a Cable Controls Remote. They are out of Louisiana. It comes with complete instruction. I can get you a phone # later. It cost about 200.00.
By
52lincoln
Date
02-06-2008 06:21
the weldtron i had never worked right
Topic
Welding Industry
/
General Welding Discussion
/ Remote amperage controls
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill