By
mvnreddy
Date
02-16-2008 12:45
What should be the hardness for P-91 material.
What should be the recomended hardness on the weldment.
What should be the hardness at the HAZ i understand the hardness is low at the HAZ by how much and why.
Kindly let me know.
By
Stephan
Date
02-16-2008 16:44
mvnreddy,
as a kind question.
Have you already tried the "Search" function by setting the Keyword "P91"?
Best,
Stephan
By
nosetackle
Date
02-18-2008 05:59
http://www.aws.org/cgi-bin/mwf/topic_show.pl?pid=87199;hl=p91#pid87199
Topic
Welding Industry
/
Technical Discussions
/ P-91 material
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill