- - By PrairieDawg (*) Date 03-01-2008 03:04
[deleted]
Parent - - By dbigkahunna (****) Date 03-01-2008 03:18
6010
Parent - By Stringer (***) Date 03-01-2008 04:49
Roger the 6010, but if it's super thin then maybe go 6013.