I agree with Dave on slag inclusions. The story I got from one of my customers is that the problem can start with a cast ingot. Apparently, once the ingot has cooled, the top portion that includes a lot of slag is removed before the good stuff is rolled. If the "bad" stuff is not removed completely, the slag gets rolled and can cause delamination.
Girish
http://www.welding-consultant.com