somebody knows how to change the voltage input in a Linde 250 mig machine?is set at 570 v and I want to change it to 220 but need some help my email is edgar12221@yahoo.com if somone is willing to help emailme I appreciate any kind of help thankyou guys.
Attachment: lindeboard.jpg (0B)
Attachment: lindeboard2.jpg (0B)
Attachment: lindeboard3.jpg (0B)
Parent - By Jeffrey Grady (***) Date 04-11-2008 04:00
efenix728,
I have a person in mind that may very well be able to help you in this endeavor. here is the info you need to contact them.

Kaye Sellon
KSELLON@BILLSWELDERREPAIR.COM
HTTP://www.billswelderrepair.com

I hope this helps you.

Respectfully, Jeffrey S. Grady
Parent - By DaveBoyer (*****) Date 04-11-2008 04:03
      The pictures You posted shows the machine to be set up for 460 V.

       To change to 230 You loosen the nuts and move the copper jumper bars to the positions marked 230.

       You will most likely need to feed the machine with larger cable, as the amperage draw will be 2x wat it was on 460 V.
Parent - By KSellon (****) Date 04-11-2008 15:18
HERE---
Attachment: LINDEVI252001.jpg (0B)
Attachment: LINDEVI252002.jpg (0B)
Attachment: LINDEVI252003.jpg (0B)
Attachment: LINDEVI252004.jpg (0B)
Attachment: LINDEVI252005.jpg (0B)
Up Topic Welding Industry / General Welding Discussion / linde machine

Powered by mwForum 2.29.2 © 1999-2013 Markus Wichitill