- - By lees Date 06-06-2001 18:00
Having problems with fixturing pieces (locator& holding pins) used in RW automated welding units. We are welding 1008 CRS parts in a nested fixture. Have steel components isolated within ceramic holders. Seeing excessive wear and arching on pins. Looking for some suggestions.
Parent - By bmaas1 (***) Date 06-11-2001 00:33
IT COULD BE A NUMBER OF THINGS. PRESSURE TOO HIGH, TIPS NOT DRESSED PROPERLY, GAPS IN MATERIAL, ETC.